Leave Your Message

Urea Formaldehyde Resin Adhesive Powder | China Suppliers & Factory Quality Products

,

Discover the high-quality Glue Mixing Ratio for Urea-formaldehyde resin powder, specially formulated for optimal performance. Our recommended mixing ratio is 100 parts resin powder to 40-60 parts water, ensuring excellent bonding and durability.

,

At our factory in China, we prioritize the quality of our products. We source premium boards and meticulously adjust their moisture content to a perfect 8-12%. Our boards undergo rigorous pretreatment, with surfaces being smooth and flat, and any imperfections such as bulges, holes, or cracks repaired thoroughly. For superior adhesion, we guarantee that the surface of the adherend is free from oil and dust.

,

As trusted suppliers in the industry, we are committed to providing reliable and effective adhesive solutions for your needs.

,

    Urea-formaldehyde resin powder

    Usage method:
    1. Glue mixing ratio

    Urea-formaldehyde resin powder : water (weight ratio)

    100 parts : 40-60 parts
    2. Board pretreatment
    • Select high-quality boards, and adjust the moisture content of the boards to 8-12%
    • The surface of the board is smooth and flat, and the convex bulges, concave holes and cracks on the surface are repaired. The surface of the adherend is oil-free and dust-free.
    • The thickness accuracy of the board is controlled within ±0.08mm
    • The board with a cured but unpressed glue layer cannot be directly coated with glue for a second time and must be sanded before use.
    3. Glue mixing process
    • Dissolve the glue powder in water according to the above water ratio and stir it into a uniform liquid. The suitable water temperature is 15-30℃. In winter, hot water can be used to mix the glue to reduce clumping (it must be stirred with a mixer for 5-10 minutes until it is uniform and free of particles before it can be used)
    • H01 drying agent is mixed according to the temperature
    4. Gluing process
    • Standard glue coating amount: 200-230g/m2, small glue lines on both sides are the best, no lack of glue.
    • The stacking time of the boards after glue coating shall not exceed 30min. When the temperature is high, the stacking time shall be shortened. It is strictly forbidden to blow the fan on the stacked boards after glue coating.
    • Do not use foaming glue
    5. Pressurization time

    Please follow standard pressurization procedures based on your equipment and board thickness.

    6. Curing

    After the pressurization time is reached, the press can be unloaded and removed from the press, but it must be stacked for 24 hours before entering the next process. If the strength is to be tested, it needs to be cured for more than 72 hours.

    (Especially for the glued products that will be subjected to intense vibration in the next process, such as sawing, sanding, drilling, etc., the necessary curing time is an indispensable process to ensure product quality.)

    Frequently Asked Questions (FAQ)

    Q1: What is the recommended mixing ratio for Urea-formaldehyde resin powder and water?
    A: The standard weight ratio is 100 parts of Urea-formaldehyde resin powder to 40-60 parts of water.
    Q2: What is the optimal moisture content for boards before applying glue?
    A: The moisture content of the selected high-quality boards should be adjusted to between 8% and 12% before processing.
    Q3: How should the glue powder be stirred and dissolved?
    A: Dissolve the powder in water (ideal temperature 15-30℃) and stir with a mixer for 5-10 minutes until the mixture is uniform and completely free of particles. In winter, hot water can be used to prevent clumping.
    Q4: What is the standard glue coating amount and maximum stacking time?
    A: The standard coating amount is 200-230g/m2. Once coated, the stacking time must not exceed 30 minutes, and the stacking time should be shortened in high-temperature environments. Avoid blowing fans directly on the stacked boards.
    Q5: How long should the glued boards cure before subsequent processing or testing?
    A: The boards must be stacked for 24 hours after press unloading before moving to the next process. If you are conducting strength testing, a curing time of more than 72 hours is required.