Product Introduction
Plywood glue refers to an adhesive used to splice wood products such as integrated materials. It is suitable for plywood bonding of non-structural materials and structural materials. The main of plywood glue is a specially made polyvinyl acetate emulsion with excellent waterproof effect, and the curing is generally isocyanate. The color is a milky white viscous liquid as the main, and the curing is light brown. The main of plywood glue can generally be used alone as a finger-joined glue.
Plywood of ebony, cherry, red oak, white oak, yellow rose, black walnut and other woods.
In line with GB18583-2008 standard; good bonding strength, water resistance, weather resistance and solvent resistance, all indicators meet international industry standards—European D4 standard and Japanese JAS standard.
Environment and wood temperature 6-35°C, wood moisture content 8-12%, curing ratio 100:15 (weight ratio), wood precision error.
Common Problems of Two-Component Plywood Glue
Insufficient curing ratio: Curing ratio should be strictly maintained at 100:10 (softwood) : 15 (hardwood).
Excessive board moisture content: The moisture content of the board is too high (standard moisture content is 8-12%, and the difference in moisture content of adjacent wood must be less than 1%).
Inadequate board precision: The board precision is not enough, uneven processing, knife marks, pollution, etc., resulting in the actual bonding surface being smaller than the required bonding surface (board precision).
Improper pressing parameters: Insufficient or uneven pressurization pressure (softwood 6-10kg/cm2, hardwood 10-15kg/cm2).
Low operational temperatures: The environment, wood, and adhesive temperature are too low (recommended above 6°C).
Frequently Asked Questions (FAQ)
The standard curing ratio by weight is 100:15 generally. For specific materials, the ratio is 100:10 for softwood and 100:15 for hardwood.
The wood moisture content should be maintained between 8% and 12%, with the difference in moisture content between adjacent wood pieces kept below 1%.
It complies with the GB18583-2008 standard and meets international performance requirements including the European D4 standard and Japanese JAS standard.
Apply a pressurization pressure of 6-10 kg/cm² for softwood and 10-15 kg/cm² for hardwood to ensure optimal bonding contact.
The operational temperature for the environment, wood, and adhesive should be between 6°C and 35°C (recommended strictly above 6°C).
Yes, the main component (milky white polyvinyl acetate emulsion) can generally be used independently as a finger-jointed glue.